You are here: Home / Technical / Applicators guide / Catalyst consumption


Acrydur catalyst consumption chart


How to cure MMA The curing time of MMA depends of the air/floor temperature.

When the temperature drops, curing time will be prolonged.


Acrydur RC quantuty for Acrydur resins.

Temperature
Degrees C
GRB1L2L3MN1N4T1
5-106%1,5%4%5%4,5%4,5%1,5%
10-155%1,5%3%4%3,5%3%1,2%
15-204%1,5%3%3%3,5%3%1,0%
20-253%1,0%2%2%2%2%0,6%
25-303%1,0%2%2%2%2%0,4%
20-352%1,0%1,5%1%1%1%0,3%
36 degrees C and above call your rep for advice. Do not proceed.

Peroxide quantity calculated on used resin. Temperature statements refer to resin-, floor- and air-temperature. NOTE: All values are derived from laboratory tests. Deviations caused by environmental factors might occur. For application below 5 degrees C please refer to seperate datasheet

 

Contact us

Please contact us if you have any questions - we are happy to help.

International Headoffice

 Tværvejen 15, DK-5580 Nr. Åby

 +45 70 21 38 88

 info@ulfcar.com